Product Description
PW-CM Deinking agent for glass
Product features:
1 It can be used repeatedly .
2 Bad printing of glass is Soaked into 8008 , the ink layer will have apparent soaking ,and will
Swell or swell off .
2 No bad effect for surface of glass will be caused if long time soaking into PW-CM Method of use:
1 Put bad printing of glass into thePW-CM solution container for 5-20 minutes ( for ink layer is
difficult to peel off , soaking time can be longer ).
2 Use blade or Wooden shovel to clear the coating or use Rags to Rub ink layer in the8008
solution container to make ink layer peel off .
3 If you use washing agent made by our company to wash the remain of glass surface , result
will be better .
4 PW-CM can be used repeatedly, if 8008 solution become dirty or muddy , 8008 solution function
won’t be effected and you can use Filter cloth Gauze(450 or 520) to filter Particle and can
continue to use PW-CM.
5 For certain kind of glass ink , pls choose the right soaking time , long soaking time may make
it difficult to clean .
Note :
1 PW-CM is irritant for skin :
(1) to avoid direct contact with PW-CM ,pls wear plastic gloves
(2) inhaling excessive 8008 may cause Respiratory tract uncomfortable ,so pls wear anti-
poison respirator when working.
2 If PW-CM is splashed into eyes , pls use water to wash immediately and if it is very serious ,pls
go to hospital to visit doctor .
3 PW-CM has volatility ,so if soaked in thePW-CMsolution container long time , pls cover the
container to avoid volatility .
4 PW-CM is inflammable , pls keep it away from fire source.
5 Pls use PW-CM at room temperature(20℃ ) . lower temperature ( especially at about 0 ℃ )
may make PW-CM function decrease.